MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Osterman & Co Osterlene® PPC20-2.7 High Crystallinity Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Product Description: PPC20-2.7 is a high crystallinity, high impact copolymer resin with medium melt flow rate and excellent processing attributes. It is designed for injection molded small and large appliance parts. Features of PPC20-2.7 include fast molding cycle, good processability, high stiffness, good heat aging resistance, high impact resistance and low warpage. Suggested uses include appliances, crates, packaging, consumer applications, industrial applications and tool/tote boxes.

Availability: North America
Features: Fast Molding Cycle; Good Processability; High Impact Resistance; High Stiffness; High Crystalline; Impact Copolymer; Low Warpage; Medium Flow
Uses: Appliances; Crates; Industrial Applications; Packaging; Tool/Tote Box
Processing Method: Injection Molding

Information provided by Osterman & Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 230 °C
20 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 24.3 MPa3520 psiStress; ISO 527-2/50
 24.4 MPa3540 psi2.0 in/min; ASTM D638
Elongation at Yield 3.4 %3.4 %Strain; ISO 527-2/50
 4.4 %4.4 %2.0 in/min; ASTM D638
Tensile Modulus 1.32 GPa191 ksiISO 527-2
Flexural Modulus 1.25 GPa181 ksi0.079 in/min; ISO 178
 1.29 GPa187 ksi0.051 in/min; ASTM D790A
 1.48 GPa214 ksi0.51 in/min; ASTM D790B
Izod Impact, Notched 1.44 J/cm2.70 ft-lb/inASTM D256A
Izod Impact, Notched (ISO)  3.99 kJ/m²
@Temperature -40.0 °C
1.90 ft-lb/in²
@Temperature -40.0 °F
ISO 180/1A
 4.62 kJ/m²
@Temperature -17.8 °C
2.20 ft-lb/in²
@Temperature 0.000 °F
ISO 180/1A
 8.40 kJ/m²
@Temperature 22.8 °C
4.00 ft-lb/in²
@Temperature 73.0 °F
ISO 180/1A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

POSTER143 / 267725

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.