A water based two component VOC free ambient temperature applied epoxy primer system designed for use on concrete. RECOMMENDED APPLICATIONS: Suitable for use on both dry and damp concrete structures. FEATURES: • Zero VOC’s • Easy application by roller Information provided by ITW Performance Polymers. |