MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Jilin Xingyun Chemical XY-1 Coking inhibitor for catalytic cracking
Categories: Other Engineering Material

Material Notes: This product is a complex multi-functional additive, developed by mechanism of slurry scaling formation at the bottom of fractionator system. Applying the product at the bottom of fractionator within the normal operation limit can effectively suppress the scaling formation. Therefore, it can prolong the life time of the slurry pipeline system, lower energy consumption, and enhance economic efficiency. The product also shows a good performance of oil solubility, moderate viscosity, and easy operation, etc. Adopting of this product in catalytic cracking has no harmful effect on product distribution.

Information provided by Jilin Xingyun Chemical Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.870 - 0.930 g/cc0.0314 - 0.0336 lb/in³GB/T 2540-81
Kinematic Viscosity <= 160 cSt<= 160 cStDynamic; GB/T 265-88
 
Thermal PropertiesMetricEnglishComments
Solidus <= -4.00 °C<= 24.8 °FGB/T 510-83
Flash Point >= 80.0 °C>= 176 °FGB/T 267-88
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.060 %<= 0.060 %GB/T260
 
Descriptive Properties
AppearanceRed brown liquid
Content<0.01%Mechanical admixture

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PJILINX057 / 317904

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.