Physical Properties | Metric | English | Comments |
---|
Specific Gravity | 1.16 g/cc | 1.16 g/cc |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Shore A | 81 | 81 |
| 60 @Temperature 23.0 °C, Time 252000 sec | 60 @Temperature 73.4 °F, Time 70.0 hour |
| 64 @Temperature 23.0 °C, Time 252000 sec | 64 @Temperature 73.4 °F, Time 70.0 hour |
| 72 @Temperature 125 °C, Time 252000 sec | 72 @Temperature 257 °F, Time 70.0 hour |
| 75 @Temperature 150 °C, Time 252000 sec | 75 @Temperature 302 °F, Time 70.0 hour |
| 76 @Temperature 100 °C, Time 252000 sec | 76 @Temperature 212 °F, Time 70.0 hour |
| 81 @Temperature 23.0 °C, Time 252000 sec | 81 @Temperature 73.4 °F, Time 70.0 hour |
| 81 @Temperature 125 °C, Time 252000 sec | 81 @Temperature 257 °F, Time 70.0 hour |
| 84 @Temperature 150 °C, Time 252000 sec | 84 @Temperature 302 °F, Time 70.0 hour |
| 84 @Temperature 100 °C, Time 252000 sec | 84 @Temperature 212 °F, Time 70.0 hour |
| 85 @Temperature 100 °C, Time 252000 sec | 85 @Temperature 212 °F, Time 70.0 hour |
| 85 @Temperature 100 °C, Time 252000 sec | 85 @Temperature 212 °F, Time 70.0 hour |
| 86 @Temperature 125 °C, Time 252000 sec | 86 @Temperature 257 °F, Time 70.0 hour |
| 86 @Temperature 100 °C, Time 252000 sec | 86 @Temperature 212 °F, Time 70.0 hour |
| 88 @Temperature 100 °C, Time 252000 sec | 88 @Temperature 212 °F, Time 70.0 hour |
| 88 @Temperature 150 °C, Time 252000 sec | 88 @Temperature 302 °F, Time 70.0 hour |
Tensile Strength | 20.43 MPa | 2963 psi |
| 8.27385 MPa @Temperature 23.0 °C, Time 252000 sec | 1200.02 psi @Temperature 73.4 °F, Time 70.0 hour |
| 9.9898 MPa @Temperature 23.0 °C, Time 252000 sec | 1448.9 psi @Temperature 73.4 °F, Time 70.0 hour |
| 18.550 MPa @Temperature 23.0 °C, Time 252000 sec | 2690.4 psi @Temperature 73.4 °F, Time 70.0 hour |
| 18.734 MPa @Temperature 150 °C, Time 252000 sec | 2717.1 psi @Temperature 302 °F, Time 70.0 hour |
| 19.265 MPa @Temperature 100 °C, Time 252000 sec | 2794.1 psi @Temperature 212 °F, Time 70.0 hour |
| 19.90 MPa @Temperature 150 °C, Time 252000 sec | 2886 psi @Temperature 302 °F, Time 70.0 hour |
| 20.511 MPa @Temperature 125 °C, Time 252000 sec | 2974.9 psi @Temperature 257 °F, Time 70.0 hour |
| 20.858 MPa @Temperature 100 °C, Time 252000 sec | 3025.2 psi @Temperature 212 °F, Time 70.0 hour |
| 21.0 MPa @Temperature 100 °C, Time 252000 sec | 3040 psi @Temperature 212 °F, Time 70.0 hour |
| 22.451 MPa @Temperature 125 °C, Time 252000 sec | 3256.3 psi @Temperature 257 °F, Time 70.0 hour |
| 22.451 MPa @Temperature 100 °C, Time 252000 sec | 3256.3 psi @Temperature 212 °F, Time 70.0 hour |
| 22.595 MPa @Temperature 125 °C, Time 252000 sec | 3277.1 psi @Temperature 257 °F, Time 70.0 hour |
| 22.595 MPa @Temperature 150 °C, Time 252000 sec | 3277.1 psi @Temperature 302 °F, Time 70.0 hour |
| 23.391 MPa @Temperature 100 °C, Time 252000 sec | 3392.6 psi @Temperature 212 °F, Time 70.0 hour |
Elongation, Ultimate | 380 % | 380 % |
| 160 % @Temperature 23.0 °C, Time 252000 sec | 160 % @Temperature 73.4 °F, Time 70.0 hour |
| 199.9 % @Temperature 23.0 °C, Time 252000 sec | 199.9 % @Temperature 73.4 °F, Time 70.0 hour |
| 229.9 % @Temperature 100 °C, Time 252000 sec | 229.9 % @Temperature 212 °F, Time 70.0 hour |
| 229.9 % @Temperature 150 °C, Time 252000 sec | 229.9 % @Temperature 302 °F, Time 70.0 hour |
| 310.1 % @Temperature 100 °C, Time 252000 sec | 310.1 % @Temperature 212 °F, Time 70.0 hour |
| 319.96 % @Temperature 150 °C, Time 252000 sec | 319.96 % @Temperature 302 °F, Time 70.0 hour |
| 340.1 % @Temperature 125 °C, Time 252000 sec | 340.1 % @Temperature 257 °F, Time 70.0 hour |
| 340.1 % @Temperature 150 °C, Time 252000 sec | 340.1 % @Temperature 302 °F, Time 70.0 hour |
| 349.98 % @Temperature 125 °C, Time 252000 sec | 349.98 % @Temperature 257 °F, Time 70.0 hour |
| 359.86 % @Temperature 100 °C, Time 252000 sec | 359.86 % @Temperature 212 °F, Time 70.0 hour |
| 359.86 % @Temperature 100 °C, Time 252000 sec | 359.86 % @Temperature 212 °F, Time 70.0 hour |
| 361.6 % @Temperature 125 °C, Time 252000 sec | 361.6 % @Temperature 257 °F, Time 70.0 hour |
| 369.5 % @Temperature 23.0 °C, Time 252000 sec | 369.5 % @Temperature 73.4 °F, Time 70.0 hour |
| 372 % @Temperature 100 °C, Time 252000 sec | 372 % @Temperature 212 °F, Time 70.0 hour |
100% Modulus | 5.52 MPa | 800 psi |
Tear Strength | 44.9 kN/m | 256 pli |
Compression Set | 19.3 % @Temperature 100 °C, Time 79200 sec | 19.3 % @Temperature 212 °F, Time 22.0 hour |
| 21.4 % @Temperature 100 °C, Time 79200 sec | 21.4 % @Temperature 212 °F, Time 22.0 hour |
| 24.4 % @Temperature 100 °C, Time 252000 sec | 24.4 % @Temperature 212 °F, Time 70.0 hour |
| 30.3 % @Temperature 100 °C, Time 252000 sec | 30.3 % @Temperature 212 °F, Time 70.0 hour |
|
Thermal Properties | Metric | English | Comments |
---|
Brittleness Temperature | -55.0 °C | -67.0 °F |
Shrinkage | -2.80 % @Temperature 100 °C, Time 252000 sec | -2.80 % @Temperature 212 °F, Time 70.0 hour |
| -2.60 % @Temperature 150 °C, Time 252000 sec | -2.60 % @Temperature 302 °F, Time 70.0 hour |
| -2.40 % @Temperature 125 °C, Time 252000 sec | -2.40 % @Temperature 257 °F, Time 70.0 hour |
| 1.6 % @Temperature 23.0 °C, Time 252000 sec | 1.6 % @Temperature 73.4 °F, Time 70.0 hour |
| 2.0 % @Temperature 100 °C, Time 252000 sec | 2.0 % @Temperature 212 °F, Time 70.0 hour |
| 13 % @Temperature 100 °C, Time 252000 sec | 13 % @Temperature 212 °F, Time 70.0 hour |
| 16.7 % @Temperature 125 °C, Time 252000 sec | 16.7 % @Temperature 257 °F, Time 70.0 hour |
| 17.6 % @Temperature 150 °C, Time 252000 sec | 17.6 % @Temperature 302 °F, Time 70.0 hour |
| 33.2 % @Temperature 23.0 °C, Time 252000 sec | 33.2 % @Temperature 73.4 °F, Time 70.0 hour |
| 56.5 % @Temperature 23.0 °C, Time 252000 sec | 56.5 % @Temperature 73.4 °F, Time 70.0 hour |
|
Descriptive Properties |
---|
Color | Black |