MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Nordic Grafting Company Acti-Tech™ 09MA13 Compatibilizer
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Acti-Tech™ compatibilizers are based on Vistamaxx™ performance polymers grafted with maleic anhydride through a highly efficient melt-grafting process. Acti-Tech compatibilizer 09MA13 is a highly versatile grade with average MFR among the Acti-Tech compatibilizers range. It is designed to enhance performance of a wide variety of polymer compounds and is particularly recommended for the following applications:
  • Compounding formulation
  • Adhesion promoter on metal or other polar substrates
  • Soft compatibilizer for polar/unpolar polymers alloys
  • Impact modifier of stiff polar engineering plastics
  • Coupling agent for WPC, natural fiber or mineral HFFR fillers
Due to the chemical nature of its polymer backbone, Acti-Tech compatibilizer 09MA13 is compatible with most polyolefins, i.e. PE, PP, EVA, EBA or POE.

Information provided by Nordic Grafting Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.890 g/ccISO 1183
Melt Flow 15 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Flexural Modulus 115 MPaISO 178
 
Descriptive Properties
Maleic anhydride content>1.0%FTIR

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BYK PRIEX® 20093 Maleic Anhydride Grafted PP homopolymer
BYK PRIEX® 15005 Maleic Anhydride modified LDPE
BYK PRIEX® 12031 Maleic Anhydride Grafted HDPE
DuPont Fusabond® MZ203D Polypropylene Impact Copolymer
DuPont Fusabond® MX110D Linear Low Density Polyethylene

PNGC002 / 238944

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.