MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Persian Gulf Polymer LDPE – LFI2047A
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: LFI2047A is a low density polyethylene, with good toughness and good optical properties. This product contains a medium level of anti-block and slip agent (Erucamide), has low energy consumption during processing and a good draw down ability. It typically exhibits low friction and low blocking. Processing Method: LFI2047A is recommended for blown film extrusion. This product is very suitable for high clarity laundry bags, textile wrapping films and zip lock bags. This grade enables high speed converting without sticking.

Property data based on 25 µm blown film produced at a melt temperature of 160°C and 3 BUR using 100% LTM 2047/37.

Information provided by Persian Gulf Polymer - Pooya Tejarat Novin Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.920 g/ccISO 1183 (A)
Melt Flow 4.7 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 12.0 MPaISO 527
Film Tensile Strength at Yield, TD 11.0 MPaISO 527
Film Elongation at Break, MD 100 %ISO 527
Film Elongation at Break, TD >= 500 %ISO 527
Secant Modulus, TD 0.200 GPaISO 527
Tensile Impact 150 J/cmASTM D4272
Coefficient of Friction 0.20ASTM D1894
Tear Strength 25.0 kN/mISO 6383-2
 80.0 kN/mMD; ISO 6383-2
Film Tensile Strength at Break, MD 27.0 MPaISO 527
 200 MPaISO 527
Film Tensile Strength at Break, TD 15.0 MPaISO 527
 
Optical PropertiesOriginal ValueComments
Haze 9.0 %
@Thickness 0.0250 mm
ASTM D1003
Gloss 55 %45°; ASTM D2457
 
Descriptive Properties
Blocking20gBased on 25 µm blown film produced at a melt temperature of 160°C and 3 BUR using 100% LTM 2047/37. SABTEC Method
Re-blocking10gSABTEC Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPERSI966 / 250370

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.