Physical Properties | Metric | English | Comments |
---|
Specific Gravity | 1.19 g/cc | 1.19 g/cc |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Shore A | 65 | 65 |
| 51 @Temperature 23.0 °C, Time 252000 sec | 51 @Temperature 73.4 °F, Time 70.0 hour |
| 53 @Temperature 23.0 °C, Time 252000 sec | 53 @Temperature 73.4 °F, Time 70.0 hour |
| 55 @Temperature 150 °C, Time 252000 sec | 55 @Temperature 302 °F, Time 70.0 hour |
| 57 @Temperature 125 °C, Time 252000 sec | 57 @Temperature 257 °F, Time 70.0 hour |
| 59 @Temperature 100 °C, Time 252000 sec | 59 @Temperature 212 °F, Time 70.0 hour |
| 62 @Temperature 23.0 °C, Time 252000 sec | 62 @Temperature 73.4 °F, Time 70.0 hour |
| 65 @Temperature 100 °C, Time 252000 sec | 65 @Temperature 212 °F, Time 70.0 hour |
| 68 @Temperature 100 °C, Time 252000 sec | 68 @Temperature 212 °F, Time 70.0 hour |
| 68 @Temperature 125 °C, Time 252000 sec | 68 @Temperature 257 °F, Time 70.0 hour |
| 69 @Temperature 150 °C, Time 252000 sec | 69 @Temperature 302 °F, Time 70.0 hour |
| 72 @Temperature 125 °C, Time 252000 sec | 72 @Temperature 257 °F, Time 70.0 hour |
| 72 @Temperature 125 °C, Time 252000 sec | 72 @Temperature 257 °F, Time 70.0 hour |
Tensile Strength | 13.98 MPa | 2027 psi |
| 5.2129 MPa @Temperature 23.0 °C, Time 252000 sec | 756.07 psi @Temperature 73.4 °F, Time 70.0 hour |
| 7.3229 MPa @Temperature 23.0 °C, Time 252000 sec | 1062.1 psi @Temperature 73.4 °F, Time 70.0 hour |
| 11.292 MPa @Temperature 23.0 °C, Time 252000 sec | 1637.8 psi @Temperature 73.4 °F, Time 70.0 hour |
| 12.844 MPa @Temperature 150 °C, Time 252000 sec | 1862.8 psi @Temperature 302 °F, Time 70.0 hour |
| 12.913 MPa @Temperature 100 °C, Time 252000 sec | 1872.9 psi @Temperature 212 °F, Time 70.0 hour |
| 13.430 MPa @Temperature 150 °C, Time 252000 sec | 1947.9 psi @Temperature 302 °F, Time 70.0 hour |
| 13.5983 MPa @Temperature 100 °C, Time 252000 sec | 1972.27 psi @Temperature 212 °F, Time 70.0 hour |
| 14.367 MPa @Temperature 125 °C, Time 252000 sec | 2083.8 psi @Temperature 257 °F, Time 70.0 hour |
| 14.689 MPa @Temperature 100 °C, Time 252000 sec | 2130.4 psi @Temperature 212 °F, Time 70.0 hour |
| 15.681 MPa @Temperature 125 °C, Time 252000 sec | 2274.3 psi @Temperature 257 °F, Time 70.0 hour |
| 15.681 MPa @Temperature 125 °C, Time 252000 sec | 2274.3 psi @Temperature 257 °F, Time 70.0 hour |
| 16.142 MPa @Temperature 125 °C, Time 252000 sec | 2341.2 psi @Temperature 257 °F, Time 70.0 hour |
Elongation, Ultimate | 410 % | 410 % |
| 150.06 % @Temperature 23.0 °C, Time 252000 sec | 150.06 % @Temperature 73.4 °F, Time 70.0 hour |
| 210.33 % @Temperature 23.0 °C, Time 252000 sec | 210.33 % @Temperature 73.4 °F, Time 70.0 hour |
| 280.03 % @Temperature 125 °C, Time 252000 sec | 280.03 % @Temperature 257 °F, Time 70.0 hour |
| 280.03 % @Temperature 125 °C, Time 252000 sec | 280.03 % @Temperature 257 °F, Time 70.0 hour |
| 280.03 % @Temperature 150 °C, Time 252000 sec | 280.03 % @Temperature 302 °F, Time 70.0 hour |
| 309.96 % @Temperature 125 °C, Time 252000 sec | 309.96 % @Temperature 257 °F, Time 70.0 hour |
| 319.8 % @Temperature 23.0 °C, Time 252000 sec | 319.8 % @Temperature 73.4 °F, Time 70.0 hour |
| 339.89 % @Temperature 100 °C, Time 252000 sec | 339.89 % @Temperature 212 °F, Time 70.0 hour |
| 339.89 % @Temperature 150 °C, Time 252000 sec | 339.89 % @Temperature 302 °F, Time 70.0 hour |
| 350.1 % @Temperature 125 °C, Time 252000 sec | 350.1 % @Temperature 257 °F, Time 70.0 hour |
| 350.1 % @Temperature 100 °C, Time 252000 sec | 350.1 % @Temperature 212 °F, Time 70.0 hour |
| 410 % @Temperature 100 °C, Time 252000 sec | 410 % @Temperature 212 °F, Time 70.0 hour |
100% Modulus | 2.54 MPa | 368 psi |
Tear Strength | 37.3 kN/m | 213 pli |
Compression Set | 7.7 % @Temperature 100 °C, Time 79200 sec | 7.7 % @Temperature 212 °F, Time 22.0 hour |
| 16.9 % @Temperature 100 °C, Time 79200 sec | 16.9 % @Temperature 212 °F, Time 22.0 hour |
| 19.8 % @Temperature 125 °C, Time 252000 sec | 19.8 % @Temperature 257 °F, Time 70.0 hour |
|
Thermal Properties | Metric | English | Comments |
---|
Brittleness Temperature | 13.3 °C | 56.0 °F |
Shrinkage | -6.10 % @Temperature 150 °C, Time 252000 sec | -6.10 % @Temperature 302 °F, Time 70.0 hour |
| -6.00 % @Temperature 100 °C, Time 252000 sec | -6.00 % @Temperature 212 °F, Time 70.0 hour |
| -5.80 % @Temperature 125 °C, Time 252000 sec | -5.80 % @Temperature 257 °F, Time 70.0 hour |
| 3.9 % @Temperature 100 °C, Time 252000 sec | 3.9 % @Temperature 212 °F, Time 70.0 hour |
| 4.2 % @Temperature 23.0 °C, Time 252000 sec | 4.2 % @Temperature 73.4 °F, Time 70.0 hour |
| 14 % @Temperature 100 °C, Time 252000 sec | 14 % @Temperature 212 °F, Time 70.0 hour |
| 16.4 % @Temperature 125 °C, Time 252000 sec | 16.4 % @Temperature 257 °F, Time 70.0 hour |
| 18.4 % @Temperature 150 °C, Time 252000 sec | 18.4 % @Temperature 302 °F, Time 70.0 hour |
| 34.9 % @Temperature 23.0 °C, Time 252000 sec | 34.9 % @Temperature 73.4 °F, Time 70.0 hour |
| 64.2 % @Temperature 23.0 °C, Time 252000 sec | 64.2 % @Temperature 73.4 °F, Time 70.0 hour |
|
Descriptive Properties |
---|
Color | Black |