MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Kalix® 5950 HFFR High Performance (HPPA), 50% glass fiber
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA)

Material Notes: 50% glass fiber, halogen-free flame retardant, low warpage

Kalix® 5950 HFFR is a halogen-free, flame retardant (UL-94 V0 at 0.4 mm), highly reinforced polyamide material specifically formulated for high strength and stiffness applications where good impact resistance and excellent dimensional stability after molding are required. The formulation also addresses warpage issues associated with the anisotropic shrinkage of glass fiber reinforced materials so that close tolerance molding is more easily achieved. Its low viscosity and excellent flow properties make the material ideal for filling parts with thin-walled sections such as those encountered in the mobile electronics industry.

- Black: Kalix® 5950 BK 000 HFFR
- White: Kalix® 5950 WH 000 HFFR
- White: Kalix® 5950 WH 001 HFFR
- White: Kalix® 5950 WH 008 HFFR

Applications: Cell Phones; Electrical Parts; Electrical/Electronic Applications; Thin-walled Parts

Features: Flame Retardant; Good Dimensional Stability; Good Impact Resistance; Good Surface Finish; Halogen Free; High Flow; High Stiffness; High Strength; Low Moisture Absorption; Low Warpage; Paintable; Platable

Typical values shown tested on Dry as Molded samples.

Standard Packaging and Labeling:
- Kalix® HFFR resin is packaged in foil lined, multiwall paper bags containing 25 kg (55 pounds) of material. Individual packages will be plainly marked with the product number, the color, the lot number, and the net weight.

Injection notes: Storage:
- Kalix® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Kalix® resins be dried prior to molding following the recommendations found in this datasheet and/or in the Kalix® processing guide.
Drying:
- Kalix® HFFR is supplied in sealed bags. It should be dried before molding because excessive moisture content will result in reduced mechanical properties and processing issues, such as excessive nozzle drooling, foaming and splay visible on the molded parts.
- Drying temperatures of up to 100°C may be used for dark colored resin (such as black) to achieve shorter drying times, if necessary. For lighter colored resin, 80°C drying temperature is recommended to minimize the risk of oxidative discoloring.
- Use of a desiccant dryer with -40°C dewpoint is strongly suggested to ensure Kalix® material has reached optimum moisture content before processing.
Injection Molding:
- Kalix® HFFR can be readily injection molded in most screw injection molding machines. A general purpose screw is recommended, with minimum back pressure. The melt temperature should be in the range 280°-285°C (535°F-545°F). Generally this can be achieved with barrel temperatures from 250°C (482°F) in the rear zone, gradually increasing to 280°C-290°C (535°F-554°F) in the front zone. Mold temperature heater set points should be in the range of 115°C-130°C (239°F-266°F) with surface finish improving as the temperature is increased.
- Set injection pressure to give rapid injection. Adjust holding pressure to one-half injection pressure. Set hold time to maximize part weight. Transfer from injection to hold pressure at the screw position just before the part is completely filled.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.68 g/ccISO 1183
Water Absorption 0.11 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.00060 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0018 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 183 MPaISO 527-2
Tensile Strength, Yield 245 MPaISO 527-2
Elongation at Break 1.8 %ISO 527-2
Tensile Modulus 20000 MPaISO 527-2
Flexural Strength 350 MPaISO 178
Flexural Modulus 19000 MPaISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²Type 1, Notch A; ISO 180
Izod Impact, Unnotched (ISO) 50.0 kJ/m²ISO 180
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 4.48
@Frequency 2.40e+9 Hz
Method B; ASTM D2250
Dissipation Factor 0.011
@Frequency 2.40e+9 Hz
Method B; ASTM D2250
Comparative Tracking Index 600 VUL 746
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 255 °CUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 247 °CUnannealed; ISO 75-2/A
Glass Transition Temp, Tg 90.0 °CDSC
Flammability, UL94 V-0
@Thickness 0.400 mm
 5VA
@Thickness 1.50 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 270 °C
Front Barrel Temperature 285 °C
Melt Temperature 275 - 285 °CInjection
Mold Temperature 115 - 130 °C
Drying Temperature 80.0 - 100 °C
@Time 14400 - 43200 sec
Moisture Content <= 0.070 %Injection
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBlack; White
FormsPellets
ProcessingInjection Molding
RoHS ComplianceYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4305 / 280105

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.