MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
KLJ Group KANATOL 800S Primary plasticizer for PVC and PVC copolymers
Categories: Fluid

Material Notes: Properties: DOP Super is almost colourless and odorless oily liquid, free of foreign materials 0 which is slightly soluble in water ( 0.285mg/L at 24 C ) but soluble in alcohols, hexane etc. It is miscible and compatible with all the monomeric plasticizers of PVC compounding.

Application: DOP Super is used as a plasticizer in PVC resins for fabricating flexible vinyl products like:- vinyl upholstery, tablecloth, shower curtain, raincoats, shoes, garden hoses, swimming pool liners, polymeric coatings, cable coating, component of paper & paperboard, defoaming agents, surface lubricants, in order of importance. The only significant non-plasticizer use for DOP is an replacement for polychlorinated biphenyls in dielectric fluid for electric capacitors. The miscellaneous use for DOP Super are:- as a solvent in erasable ink, as an acaricide for use in orchards, as an inert ingredient in pesticides, as a vacuum pump oil, in detecting leaks in respirators. Apart from above applications, DOP Super is more suitable for medical & food grade applications like:- Drinking water bottle, Toys, Disposable syringes and many medical appliances.

Chemical Name: DOP

Molecular Formula: C 24 H38 O 4

Molecular Structure: C 4 H9 ( C2 H 5 )C2 H3 -CO2 -C6 H4 -CO2 - C2 H 9 ( C2 H 5 )C4 H9

CAS Number: 117-81-7

UN. NO: 3082

EINECS NO: 204-211-0

Information provided by KLJ Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.980 - 0.986 g/cc
@Temperature 27.0 °C
ASTM-D-1045-86
Viscosity 80 - 84 cP
Molecular Weight 390 g/mol
 
Thermal PropertiesOriginal ValueComments
Boiling Point 231 °C
@Pressure 0.700 MPa
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.484 - 1.488
@Temperature 27.0 °C
ASTM-D-1045-86
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.050 %ASTM-E-203
Shelf Life 24.0 Month
 
Descriptive Properties
Acidity after heat treatment0.00015ASTM-D-1045-86
Acidity as Acid<0.0033%ASTM-D-1045-86
Color<15 HUASTM-D-1045-86
Content<0.03%Residual alcohol
 >99.9Ester Content, ASTM-D-1045-86
 >99.9%Plasticizing Ester, ASTM-D-1045-86
 284-290 mg KOH/gEster Value, ASTM-D-1045-86

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKLJ341 / 284362

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.