MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials RCH® 500 High Molecular Weight Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Extruded

Material Notes: RCH 500 High Molecular Weight HMW-PE is a highly versatile, high-molecular weight plastic that is ideal for many orthotic applications. It has a forming temperature between +160°C to 170°C , is suited for deep-drawing and is both malleable and weldable. RCH 500 is commonly used for ankle foot orthoses, body jackets and upper limborthoses.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.960 g/ccISO 1183-1
Water Absorption 0.10 %
@Time 86400 sec
Immersion; ISO 62
Water Absorption at Saturation 0.10 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 62ISO 868
Tensile Strength, Ultimate 20.0 MPaISO 527-1/-2
Elongation at Break 50 %ISO 527-1/-2
Modulus of Elasticity 0.800 GPaISO 527-1/-2
Charpy Impact Unnotched NBISO 179-1/1eU
Charpy Impact, Notched 1.50 J/cm²ISO 179-1/1eA
Sand Slurry 400based on TIVAR®1000 = 100; ISO 15527
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 1.00e+12 ohmANSI/ESD STM 11.11
 
Thermal PropertiesOriginal ValueComments
CTE, linear 200 µm/m-°C
@Temperature 23.0 - 100 °C
Melting Point 135 °CDSC, 10°C / min; ISO 11357-1/-3
Maximum Service Temperature, Air 80.0 °CContinuous (20.000 hrs)
Minimum Service Temperature, Air -30.0 °C
Flammability, UL94 HB
@Thickness 3.00 mm
 
Descriptive Properties
ColorWhite, Black, colors

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

P1SM940 / 320677

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.