Physical Properties | Metric | English | Comments |
---|
Specific Gravity | 1.22 g/cc | 1.22 g/cc |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Shore A | 78 | 78 |
| 67 @Temperature 23.0 °C, Time 252000 sec | 67 @Temperature 73.4 °F, Time 70.0 hour |
| 69 @Temperature 23.0 °C, Time 252000 sec | 69 @Temperature 73.4 °F, Time 70.0 hour |
| 73 @Temperature 125 °C, Time 252000 sec | 73 @Temperature 257 °F, Time 70.0 hour |
| 74 @Temperature 150 °C, Time 252000 sec | 74 @Temperature 302 °F, Time 70.0 hour |
| 75 @Temperature 100 °C, Time 252000 sec | 75 @Temperature 212 °F, Time 70.0 hour |
| 76 @Temperature 100 °C, Time 252000 sec | 76 @Temperature 212 °F, Time 70.0 hour |
| 78 @Temperature 23.0 °C, Time 252000 sec | 78 @Temperature 73.4 °F, Time 70.0 hour |
| 80 @Temperature 125 °C, Time 252000 sec | 80 @Temperature 257 °F, Time 70.0 hour |
| 80 @Temperature 150 °C, Time 252000 sec | 80 @Temperature 302 °F, Time 70.0 hour |
| 82 @Temperature 100 °C, Time 252000 sec | 82 @Temperature 212 °F, Time 70.0 hour |
| 82 @Temperature 100 °C, Time 252000 sec | 82 @Temperature 212 °F, Time 70.0 hour |
| 86 @Temperature 125 °C, Time 252000 sec | 86 @Temperature 257 °F, Time 70.0 hour |
| 86 @Temperature 125 °C, Time 252000 sec | 86 @Temperature 257 °F, Time 70.0 hour |
Tensile Strength | 15.95 MPa | 2314 psi |
| 7.5339 MPa @Temperature 23.0 °C, Time 252000 sec | 1092.7 psi @Temperature 73.4 °F, Time 70.0 hour |
| 10.1949 MPa @Temperature 23.0 °C, Time 252000 sec | 1478.65 psi @Temperature 73.4 °F, Time 70.0 hour |
| 14.359 MPa @Temperature 150 °C, Time 252000 sec | 2082.6 psi @Temperature 302 °F, Time 70.0 hour |
| 15.0610 MPa @Temperature 150 °C, Time 252000 sec | 2184.42 psi @Temperature 302 °F, Time 70.0 hour |
| 15.3322 MPa @Temperature 125 °C, Time 252000 sec | 2223.75 psi @Temperature 257 °F, Time 70.0 hour |
| 15.3322 MPa @Temperature 125 °C, Time 252000 sec | 2223.75 psi @Temperature 257 °F, Time 70.0 hour |
| 15.348 MPa @Temperature 100 °C, Time 252000 sec | 2226.1 psi @Temperature 212 °F, Time 70.0 hour |
| 15.364 MPa @Temperature 125 °C, Time 252000 sec | 2228.4 psi @Temperature 257 °F, Time 70.0 hour |
| 16.3533 MPa @Temperature 23.0 °C, Time 252000 sec | 2371.85 psi @Temperature 73.4 °F, Time 70.0 hour |
| 16.8160 MPa @Temperature 100 °C, Time 252000 sec | 2438.96 psi @Temperature 212 °F, Time 70.0 hour |
| 16.911 MPa @Temperature 100 °C, Time 252000 sec | 2452.8 psi @Temperature 212 °F, Time 70.0 hour |
| 17.629 MPa @Temperature 125 °C, Time 252000 sec | 2556.9 psi @Temperature 257 °F, Time 70.0 hour |
Elongation, Ultimate | 173 % | 173 % |
| 116.1 % @Temperature 125 °C, Time 252000 sec | 116.1 % @Temperature 257 °F, Time 70.0 hour |
| 116.1 % @Temperature 125 °C, Time 252000 sec | 116.1 % @Temperature 257 °F, Time 70.0 hour |
| 120.93 % @Temperature 23.0 °C, Time 252000 sec | 120.93 % @Temperature 73.4 °F, Time 70.0 hour |
| 129.1 % @Temperature 150 °C, Time 252000 sec | 129.1 % @Temperature 302 °F, Time 70.0 hour |
| 140.95 % @Temperature 23.0 °C, Time 252000 sec | 140.95 % @Temperature 73.4 °F, Time 70.0 hour |
| 141 % @Temperature 150 °C, Time 252000 sec | 141 % @Temperature 302 °F, Time 70.0 hour |
| 147.9 % @Temperature 100 °C, Time 252000 sec | 147.9 % @Temperature 212 °F, Time 70.0 hour |
| 157.1 % @Temperature 125 °C, Time 252000 sec | 157.1 % @Temperature 257 °F, Time 70.0 hour |
| 162.966 % @Temperature 125 °C, Time 252000 sec | 162.966 % @Temperature 257 °F, Time 70.0 hour |
| 166.95 % @Temperature 100 °C, Time 252000 sec | 166.95 % @Temperature 212 °F, Time 70.0 hour |
| 173 % @Temperature 100 °C, Time 252000 sec | 173 % @Temperature 212 °F, Time 70.0 hour |
| 174.9 % @Temperature 23.0 °C, Time 252000 sec | 174.9 % @Temperature 73.4 °F, Time 70.0 hour |
100% Modulus | 7.198 MPa | 1044 psi |
Tear Strength | 34.5 kN/m | 197 pli |
| 45.6 kN/m | 260 pli |
Compression Set | 9.0 % @Temperature 100 °C, Time 79200 sec | 9.0 % @Temperature 212 °F, Time 22.0 hour |
| 9.9 % @Temperature 100 °C, Time 252000 sec | 9.9 % @Temperature 212 °F, Time 70.0 hour |
| 12 % @Temperature 125 °C, Time 79200 sec | 12 % @Temperature 257 °F, Time 22.0 hour |
| 12.9 % @Temperature 100 °C, Time 79200 sec | 12.9 % @Temperature 212 °F, Time 22.0 hour |
| 16 % @Temperature 100 °C, Time 252000 sec | 16 % @Temperature 212 °F, Time 70.0 hour |
| 20.3 % @Temperature 125 °C, Time 79200 sec | 20.3 % @Temperature 257 °F, Time 22.0 hour |
|
Thermal Properties | Metric | English | Comments |
---|
Brittleness Temperature | -37.2 °C | -35.0 °F |
Shrinkage | -4.80 % @Temperature 125 °C, Time 252000 sec | -4.80 % @Temperature 257 °F, Time 70.0 hour |
| -4.60 % @Temperature 150 °C, Time 252000 sec | -4.60 % @Temperature 302 °F, Time 70.0 hour |
| -4.60 % @Temperature 100 °C, Time 252000 sec | -4.60 % @Temperature 212 °F, Time 70.0 hour |
| -0.700 % @Temperature 23.0 °C, Time 252000 sec | -0.700 % @Temperature 73.4 °F, Time 70.0 hour |
| 2.8 % @Temperature 100 °C, Time 252000 sec | 2.8 % @Temperature 212 °F, Time 70.0 hour |
| 7.8 % @Temperature 100 °C, Time 252000 sec | 7.8 % @Temperature 212 °F, Time 70.0 hour |
| 9.2 % @Temperature 125 °C, Time 252000 sec | 9.2 % @Temperature 257 °F, Time 70.0 hour |
| 9.6 % @Temperature 150 °C, Time 252000 sec | 9.6 % @Temperature 302 °F, Time 70.0 hour |
| 23.8 % @Temperature 23.0 °C, Time 252000 sec | 23.8 % @Temperature 73.4 °F, Time 70.0 hour |
| 43.3 % @Temperature 23.0 °C, Time 252000 sec | 43.3 % @Temperature 73.4 °F, Time 70.0 hour |
|
Descriptive Properties |
---|
Color | Black |