MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Hexcel® HexPly® M81 Epoxy Resin Matrix
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: HexPly® M81 is a high performance tough epoxy matrix for use in industrial applications requiring good impact resistance and damage tolerance, such as the automotive industry. HexPly® M81 is based on the highly successful HexPly® 8552 toughened epoxy resin system, used widely around the world for the manufacture of aircraft structures. Non-aerospace customers now have the opportunity to benefit from the excellent performance of this resin system presented with reinforcements specially adapted for industrial markets.

Benefits and Features

  • Toughened epoxy matrix with excellent mechanical properties
  • Elevated temperature performance (Tg up to 200°C)
  • Versatile cure cycle (from 135°C to 180°C)
  • Available on various reinforcements
  • Excellent drape and tack

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.30 g/cc
Viscosity 3.00e+6 cP
@Temperature 65.0 °C
EN 6043-A, 2°C/min
 1.00e+9 cP
@Temperature 5.00 °C
EN 6043-A, 2°C/min
 1.00e+10 cP
@Temperature 85.0 °C
EN 6043-A, 2°C/min
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg <= 140 °Cafter ageing, Tg onset wet
 <= 200 °Conset dry
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 170 °C
 2.00 hour
@Temperature 135 °C
 2.00 hour
@Temperature 150 °C
 2.00 hour
@Temperature 180 °C
 3.00 hour
@Temperature 135 °C
 3.00 hour
@Temperature 135 °C
Gel Time 20.0 min
@Temperature 177 °C
hot plate
 50.0 min
@Temperature 145 °C
hot plate
 110 min
@Temperature 130 °C
hot plate
Shelf Life 12.0 Month
@Temperature -18.0 °C
 
Descriptive Properties
ColorYellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHEXCB9165 / 322321

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.