MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
ASI® MP 5404-FS Epoxy Adhesive
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: MP 5404-FS is a one component, heat curable thixotropic paste epoxy adhesive. It is a non-sag adhesive, which forms strong bonds to metals and ceramics. MP 5404-FS has exceptional thermal stability and resistance to water, humidity and solvents. This product offers high heat resistance and cures in less than 20 seconds via induction or infrared heating.

Information provided by Adhesive Systems, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.41 g/cc
@Temperature 25.0 °C
Viscosity 500000 - 700000 cP
@Temperature 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85
@Temperature 25.0 °C
Tensile Strength 6300 psi
Elongation at Break >= 1.5 %
Adhesive Bond Strength 3000 psiLap Shear
Izod Impact, Notched 0.360 ft-lb/in
 
Thermal PropertiesOriginal ValueComments
CTE, linear 57.2 µm/m-°C
Thermal Conductivity 19.6 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 400 °F
Minimum Service Temperature, Air -40.0 °F
Glass Transition Temp, Tg 148 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 min
@Temperature 149 °C
 7.00 min
@Temperature 121 °C
 <= 20.0 sec
@Temperature 204 °C
 30.0 sec
@Temperature 177 °C
Shelf Life 0.500 Month
@Temperature 38.0 °C
 6.00 Month
@Temperature 24.0 °C
 12.0 Month
@Temperature <=0.000 °C
Store in a cool, dry area
 
Descriptive Properties
Color / appearancegray
Press Flow60-80 sec
Sag Resistance0.315"-0.4"
Unleaded Gasoline Resistance100% strength retained after 1500 hrs of submersion.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASINC9103 / 233470

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.