System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Polytek Poly-Optic® 1490 Rigid Clear Polyurethane
Categories:
Polymer
;
Thermoset
;
Polyurethane, TS
Material Notes:
A versatile, clear polyurethane. A matte finish will give a frosted appearance, and a higher gloss will increase its transparency.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.07
g/cc
Brookfield Viscosity
690
cP
Mixed
Linear Mold Shrinkage
0.0070
in/in
Mechanical Properties
Original Value
Comments
Hardness, Shore D
80
Tensile Strength
6605
psi
8744
psi
Post cured for 16 hours at 160°F
Elongation at Break
7.7 %
12.1 %
Post cured for 16 hours at 160°F
Modulus of Elasticity
128.8
ksi
Post cured for 16 hours at 160°F
96260
ksi
Flexural Strength
10850
psi
10780
psi
@Strain 5.0 %
Post cured for 16 hours at 160°F
Flexural Modulus
282600
psi
Post cured for 16 hours at 160°F
324000
psi
Thermal Properties
Original Value
Comments
Deflection Temperature at 0.46 MPa (66 psi)
165
°F
207
°F
Post cured for 16 hours at 160°F
Processing Properties
Original Value
Comments
Cure Time
7.00
hour
Pot Life
9.00
min
Descriptive Properties
Color / Appearance
Water clear
Part A
Water clear / slight yellow
Part B
Demold Time (hrs)
1
Max Exotherm (°F)
235
1-lb mass
Mix Ratio by volume
1 to 1
Part A to Part B
Mix Ratio by weight
100 to 90
Part A to Part B
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PPOLYT9913 / 287693
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.