MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Henkel Loctite® SI 5421 Silicone
Categories: Polymer; Thermoset; Silicone

Material Notes: Chemical Type: Alkoxy silicone

Appearance (uncured): Tan Paste

Cure: Room temperature vulcanizing (RTV)

Components: One Components - requires no mixing

Application: Bonding or Gasketing

Flexibility: Enhances load bearing & shock absorbing characteristics of the bond area.

LOCTITE SI 5421 is used for automotive sensor bonding and gasketing of EMI/RF shielded enclosures. It cures to make a flexible, formed-in-place, electrically conductive bond.

Information provided by Loctite®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 3.05 - 3.30 g/cc3.05 - 3.30 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 50 - 6550 - 65Cured for 72 hours @ 25 °C / 50±5 % RH; ISO 37
Tensile Strength >= 0.700 MPa>= 102 psiCured for 72 hours @ 25 °C / 50±5 % RH; ISO 37
Elongation at Break >= 40 %>= 40 %Cured for 72 hours @ 25 °C / 50±5 % RH; ISO 37
Shear Strength >= 0.400 MPa>= 58.0 psiLap, Cured for 7 days @ 25 °C / 50±5 %, Alclad to Alclad; ISO 4587
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 0.010 ohm-cm<= 0.010 ohm-cmCured for 24 hours @ 25±2 °C / 50±5% RH; IEC 60093

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLOCT5118 / 255329

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.