MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Chengdu Letain LTP ZC-1600B PPS
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: It is required that the friction factor is low and self-lubrication is good under elevated temperature for automobile parts such as change gear, shaft bearing, axile bush, electric brush and universal joint bulb. LTP ZW-3160 serials of LETIAN Plastics is a kind of PPS/PEEK/PTFE alloy, and its wear resistant property is remarkably improved comparing to common blend materials reinforce by 30% glass fiber. The Pv value can reach to 2200 at 23?. As shown in table4 and 5.

Information provided by Chengdu Letain Plastic

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.65 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 165 MPa
Elongation at Break 0.80 %
Flexural Strength 240 MPa
Flexural Modulus 16.0 GPa
Izod Impact, Notched (ISO) 10.2 kJ/m²
Izod Impact, Unnotched (ISO) 55.0 kJ/m²
Abrasion 0.00062
@Temperature 23.0 °C
 0.00114
@Temperature 85.0 °C
 0.00125
@Temperature 150 °C
 
Thermal PropertiesOriginal ValueComments
Heat Distortion Temperature 260 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHENGLT046 / 255899

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.