DAI-EL® G-EXP-045 is a cure incorporated terpolymer with medium Mooney viscosity. It is designed for compression molding of O-rings, seals, and other parts where exceptional fluid resistance and low compression set are required. Typical Applications: O-rings, seals, gaskets, molded tubing Rheological Properties MDR 2000: Temperature: 177°C Frequency: 100 cpm Strain: 0.5° Test time: 6 min Information provided by Daikin. |