MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Dow Dow™ DGDB-5004 NT 7 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Product Description: Dow HDPE DGDB-5004 NT 7 resin is a multi-purpose polymer designed for sheet extrusion and thermoforming application, including single-serve disposables and other thin walled containers including food service such as cups, plates, bowls and refrigerated dairy containers.
Main Characteristics:
  • Maximum rigidity
  • Excellent color consistency
  • High Melt Strength
  • High Impact Strength including low temperature toughness
  • Good Top Load Strength
  • Optimized Shear Rheology for Good Processability
Complies with: US FDA 21 CFR 177.1520©2.2;Canadian HPFB No Objection. Consult the regulations for complete details.

Availability: Latin America; North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: FDA 21 CFR 177.1520© 2.2; HPFB (Canada) No Objection

Form: Pellets

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.963 g/ccASTM D792
Melt Flow 0.80 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 57 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 66ASTM D2240
Tensile Strength at Break 3500 psiASTM D638
Tensile Strength, Yield 4600 psiASTM D638
Elongation at Break 1000 %ASTM D638
Elongation at Yield 7.0 %ASTM D638
Flexural Modulus 188000 psi2% Secant; ASTM D790B
 
Thermal PropertiesOriginal ValueComments
Melting Point 271 °F
Crystallization Temperature 248 °F
Deflection Temperature at 0.46 MPa (66 psi) 169 °FUnannealed; ASTM D648
Vicat Softening Point 268 °FASTM D1525
Brittleness Temperature <= -105 °FASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDOWF439 / 311132

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.