MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BASF Ultramid® C 218 V33 BLACK 21N Nylon 6, 33% Glass Fiber Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled; Nylon 6, Heat Stabilized

Material Notes: Product Description: Ultramid® C 218 V33 BLACK 21N is a polyamid 6, reinforced with 33% of glass fiber, heat stabilized, for injection molding. The product offers an excellent combination between thermal and mechanical properties.

Availability: North America

Filler/Reinforcement: Glass Fiber, 33% Filler by Weight

Additive: Heat Stabilizer

Features: Good Dimensional Stability; Good Flow; Good Mold Release

Uses: Automotive Applications; Consumer Applications; Electrical/Electronic Applications; General Purpose; Industrial Applications; White Goods & Small Appliances

Processing Method: Injection Molding

Resin ID (ISO 1043): PA6-GF33

Information provided by BASF Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.38 g/ccISO 1183
Water Absorption 1.0 %
@Time 86400 sec
ISO 62
Maximum Moisture Content 0.20
Linear Mold Shrinkage, Flow 0.0070 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0025 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 25400 psiISO 527-2
Elongation at Break 3.1 %ISO 527-2
Tensile Modulus 1.48e+6 psiISO 527-1
Flexural Modulus 1.31e+6 psiISO 178
Izod Impact, Notched (ISO) 7.10 ft-lb/in²ISO 180/A
Charpy Impact Unnotched 38.0 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 5.70 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 62631-3-1
Dielectric Constant 2.5
@Frequency 1e+6 Hz
IEC 62631-2-1
Dissipation Factor 0.023
@Frequency 1e+6 Hz
IEC 62631-2-1
Comparative Tracking Index 400 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 406 °FUnannealed; ISO 75-2/A
Flammability, UL94 HB
@Thickness 1.52 mm
IEC 60695-11-10,-20
Glow Wire Flammability Index 1200 °F
@Thickness 1.52 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 437 - 446 °F
Middle Barrel Temperature 446 - 464 °F
Front Barrel Temperature 464 - 482 °F
Mold Temperature 176 - 212 °F
Drying Temperature 176 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBASG2057 / 310750

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.