MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Momentive Performance Materials Silopren LSR 3366/50 Liquid Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: Silopren LSR 3366/50 is a two-component liquid silicone rubber for injection molding processes. Silopren LSR 3366/50 shows an excellent aging resistance after long term exposure to high temperatures and retains very good compression set also without post-curing under these conditions. This material is an excellent candidate to consider for the manufacture of elastomeric articles requiring self- lubricating properties. The self-lubricating effect is achieved by a fluid which exudes out of the vulcanizate over an extended period of time. It typically starts between a few hours and one day after vulcanization. Vulcanizates consisting of Silopren LSR 3366/50 liquid silicone rubber are typically distinguished by the following properties: ultra-low long-term compression set without post-cure, self-lubricating properties, low viscosity, fast cure, very high thermal stability, possible to color.

Applications: single wire seals, peripheral / radial seals.

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/ccCured; DIN 53 479 A
Viscosity 220000 cPy° = 10 s-1 at 20°C.; DIN 53018
 350000 cPy° = 10 s-1 at 20°C.; DIN 53018
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 52DIN 53 505
Tensile Strength 8.60 MPaDIN 53 504 S2
Elongation at Break 450 %DIN 53 504 S2
100% Modulus 2.20 MPaDIN 53 504 S2
200% Modulus 3.90 MPaDIN 53 504 S2
300% Modulus 5.60 MPaDIN 53 504 S2
Tear Strength 40.8 kg(f)/cmASTM D 624
Compression Set 11 %
@Temperature 175 °C,
Time 79200 sec
DIN 53 517
 18 %
@Temperature 175 °C,
Time 605000 sec
DIN 53 517
 31 %
@Temperature 175 °C,
Time 3.629e+6 sec
DIN 53 517
 
Processing PropertiesOriginal ValueComments
Processing Temperature 175 °C
@Time 601 sec
Vulcanization as Tested; Die B
 
Descriptive Properties
ColorWhiteA-component
 WhitishB-component
Fluid Content (%)3A-component
 3B-component
Mix Ratio1:1 A:BAs Tested

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMOMEN9965 / 265780

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.