MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Alliance BIS-3 Injection Molded Samarium Cobalt Bonded Magnet
Categories: Ceramic; Oxide; Metal; Electronic/Magnetic Alloy

Material Notes: Injection Molded Samarium Cobalt Bonded Magnets can be made by combining SmCo powders with Nylon 6, Nylon 12, PPS and other resins. The ratios between magnetic powders and resins are endless, therefore many grades exist depending on magnetic performance, temperature resistance, and mechanical strength. These materials can be molded directly over or into another polymer or metal component. The shapes and sizes are endless, as are the magnetization patterns that can be achieved either in the molding tool or by utilizing a magnetizing fixture.

Information provided by Alliance LLC.

Key Words: Permanent SmCo Magnet
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 3.00 - 5.80 g/cc0.108 - 0.210 lb/in³
Water Absorption 0.020 - 0.050 %0.020 - 0.050 %PPS
 0.050 - 3.2 %0.050 - 3.2 %PA12
 0.30 - 11 %0.30 - 11 %PA6
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 88 - 13188 - 131
Tensile Strength, Yield 18.0 - 145 MPa2610 - 21000 psiPA6
 13.0 - 150 MPa1890 - 21800 psiPPS
 12.0 - 171 MPa1740 - 24800 psiPA12
 
Electrical PropertiesMetricEnglishComments
Magnetic Coercive Force, Hc 2500 - 3500 Oe2500 - 3500 Oe
 8000 - 15000 Oe8000 - 15000 OeIntrinsic
Magnetic Remanence, Br 3000 - 4000 Gauss3000 - 4000 Gauss
Magnetic Maximum Energy Product, BH 2.5 - 3.5 MGOe2.5 - 3.5 MGOe
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air <= 120 °C<= 248 °FPA12
 <= 150 °C<= 302 °FPA6
 <= 180 °C<= 356 °FPPS
 
Processing PropertiesMetricEnglishComments
Mold Temperature 20.0 - 150 °C68.0 - 302 °FPA12
 70.0 - 120 °C158 - 248 °FPA6
 135 - 175 °C275 - 347 °FPPS
 
Descriptive Properties
Reversible Temperature Coefficients-0.035Bd. %/°C
 -0.29Hd. %/°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NALLIAN9900 / 268436

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.