MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SCIGRIP MP100 Metal Primer
Categories: Other Engineering Material; Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: SCIGRIP® MP100 Metal Primer is a surface treatment that is designed to clean, chemically convert and prepare stainless steel and aluminum surfaces1 for permanent bonding with SCIGRIP Methacrylate Structural Adhesives. It significantly improves the long-term durability of adhesive bonds that are subjected to humid or corrosive environments such as salt water or salt spray.

MP100 Metal Primer is recommended with SG100, SG200, SG230 HV, SG600, SG745 and SG747 for metal bonding. A thin film of the metal primer is brushed or wiped on metal surfaces and allowed to dry completely before application of adhesive.

Information provided by SCIGRIP Americas.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.780 g/cc
 
Processing PropertiesOriginal ValueComments
Cure Time 5.00 - 10.0 min
@Temperature 22.0 °C
Dry Time
Shelf Life 12.0 Month
 
Descriptive Properties
ColorRed
FormWater-thin liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSCIGR950 / 243174

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.