MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Vinnolit® S 4080 Suspension PVC
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Vinnolit® S 4080 Suspension PVC for thermoplastic processing of PVC. Vinnolit® S 4080 is a specialty product for flexible PVC articles with excellent mechanical performance, primarily at elevated service temperatures. Vinnolit® S 4080 is a free-flowing powder with porous particles. It may be processed with all standard additives such as plasticizers, stabilizers, lubricants, fillers and pigments, similarly to S-PVC with a low K-value. Vinnolit® S 4080 is mixed by the standard hot or cold mixing methods. Recommended temperatures are 120 °C in the heating mixer and 40 °C in the cooling mixer. It can be processed in the form of a blend or granules on all standard equipment, such as extruders, injection molding machines and colanders.

Information provided by Vinnolit.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 0.30 %ISO 1269
Apparent Bulk Density 0.450 g/ccISO 60
Particle Size >= 63 µm>= 90% Retained on 0.063 mm Sieve; ISO 4610
 <= 250 µm<=1% Retained on 0.25 mm Sieve; ISO 4610
Viscosity Test 1.68 dl/gReduced Viscosity; ISO 1628-2
 
Descriptive Properties
K-Value80ISO 1628-2
Plasticizer Absorption (%)34ISO 4608. At room temperature.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PVINNO909 / 291106

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.