MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Pressure Seal 9718 Fluorinated Hydrocarbon
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Compound 9718 is a 70 durometer black colored Fluorinated Hydrocarbon elastomer, it is internally lubricated with Teflon to provide internal lubrication. It exhibits good resistance to heat, compression set, petroleum based oils, aliphatic and aromatic fuels. This compound contains greater than 10% Teflon by weight.

This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 2 HK 710 A1-10 B37 B38 EO78; 4 HK 710 A1-11 B38 EO78; 6 HK 710 A1-10 A1-11 B31 EO88

Information provided by Pressure Seals Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.89 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 71
 60
@Temperature 200 °C,
Time 252000 sec
Stauffer Blend 7700
 61
@Temperature 200 °C,
Time 252000 sec
Service Fluid 101
 67
@Temperature 150 °C,
Time 252000 sec
ASTM Oil #3
 68
@Temperature 23.0 °C,
Time 252000 sec
ASTM Reference Fuel C
 69
@Temperature 150 °C,
Time 252000 sec
ASTM Oil #1
 69
@Temperature 100 °C,
Time 252000 sec
Distilled water aged
 70
@Temperature 275 °C,
Time 252000 sec
Heat Aged
 71
@Temperature 23.0 °C,
Time 252000 sec
ASTM Reference Fuel A
 71
@Temperature 250 °C,
Time 252000 sec
Heat Aged
Tensile Strength 1187 psi
 720.5 psi
@Temperature 200 °C,
Time 252000 sec
Stauffer Blend 7700
 764.4 psi
@Temperature 23.0 °C,
Time 252000 sec
ASTM Reference Fuel C
 864.1 psi
@Temperature 200 °C,
Time 252000 sec
Service Fluid 101
 971 psi
@Temperature 275 °C,
Time 252000 sec
Heat Aged
 1048.1 psi
@Temperature 150 °C,
Time 252000 sec
ASTM Oil #3
 1054.1 psi
@Temperature 23.0 °C,
Time 252000 sec
ASTM Reference Fuel A
 1077.8 psi
@Temperature 150 °C,
Time 252000 sec
ASTM Oil #1
 1109.8 psi
@Temperature 100 °C,
Time 252000 sec
Distilled water aged
 1111 psi
@Temperature 250 °C,
Time 252000 sec
Heat Aged
Elongation, Ultimate 275 %
 234 %
@Temperature 200 °C,
Time 252000 sec
Stauffer Blend 7700
 262.9 %
@Temperature 250 °C,
Time 252000 sec
Heat Aged
 270.9 %
@Temperature 150 °C,
Time 252000 sec
ASTM Oil #3
 270.9 %
@Temperature 200 °C,
Time 252000 sec
Service Fluid 101
 271.1 %
@Temperature 23.0 °C,
Time 252000 sec
ASTM Reference Fuel A
 284.1 %
@Temperature 275 °C,
Time 252000 sec
Heat Aged
 284.1 %
@Temperature 150 °C,
Time 252000 sec
ASTM Oil #1
 312.1 %
@Temperature 23.0 °C,
Time 252000 sec
ASTM Reference Fuel C
 312.9 %
@Temperature 100 °C,
Time 252000 sec
Distilled water aged
100% Modulus 408 psi
Tear Strength 116 pliDie B
Compression Set 8.5 %
@Temperature 23.0 °C,
Time 79200 sec
Plied
 10.2 %
@Temperature 175 °C,
Time 79200 sec
Plied
 16.7 %
@Temperature 200 °C,
Time 79200 sec
Plied
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature 0.000 °F
Shrinkage -0.100 %
@Temperature 150 °C,
Time 252000 sec
Volume, ASTM Oil #1
 0.10 %
@Temperature 23.0 °C,
Time 252000 sec
Volume, ASTM Reference Fuel A
 1.2 %
@Temperature 150 °C,
Time 252000 sec
Volume, ASTM Oil #3
 1.8 %
@Temperature 250 °C,
Time 252000 sec
Volume, Heat Aged
 3.1 %
@Temperature 275 °C,
Time 252000 sec
Volume, Heat Aged
 3.4 %
@Temperature 100 °C,
Time 252000 sec
Volume, Distilled water aged
 4.1 %
@Temperature 23.0 °C,
Time 252000 sec
Volume, ASTM Reference Fuel C
 11.6 %
@Temperature 200 °C,
Time 252000 sec
Volume, Service Fluid 100
 19.8 %
@Temperature 200 °C,
Time 252000 sec
Volume, Stauffer Blend 7700
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPRESL118 / 318328

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.