MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Polytek Poly Wax 15 Hard Wax Blend for Carving & Casting
Categories: Other Engineering Material

Material Notes: Description: Poly Wax 15 is a white, hard, low shrinkage, mineral-filled wax, which can be cast and carved. When cast, it replicates the mold surface in detail and finish. Tool cuts are smooth and lustrous. Dull surfaces can be hand polished with a soft cloth to a satin luster.

Product Line Features:

  • Ideal for prototypes
  • Suitable for master models
  • Smooth and lustrous surfaces
  • Cast carving blanks from rubber molds of rough originals

Information provided by Polytek

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 116 cP
 
Processing PropertiesOriginal ValueComments
Processing Temperature 210 - 280 °FUse Temperature
 
Descriptive Properties
Specific Volume19.5 in³/lb
 21.6 in³/lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPTK5112 / 251104

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.