MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Formosa Plastics Formolene® FC100BR LDPE Film Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Clarity LDPE Resin with 750 ppm Slip and 1000 ppm antiblock Formolene® FC100BR is a low density polyethylene offering good balance of optical and mechanical properties. Formolene® FC100BR is formulated with slip and antiblock for use in film applications offering excellent extrusion processing and film optical properties.

Suggested Applications: Blend Partner, Light Duty Shrink, Film Mail Bags, Cast Film, Freezer Film, Produce Bags, Food Packaging, Lamination Film, Shoppers Foams Compounding, Textile Packaging, Liners Form Fill And Seal Packaging.

Information provided by Formosa Plastics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.923 g/ccASTM D1505
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
Condition E; ASTM D1238
Antiblock Level 1000 ppm
Slip Level 750 ppm
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 1600 psiASTM D882
Film Tensile Strength at Yield, TD 1600 psiASTM D882
Film Elongation at Break, MD 550 %ASTM D882
Film Elongation at Break, TD 670 %ASTM D882
Elmendorf Tear Strength, MD 120 g/milASTM D1922
Elmendorf Tear Strength, TD 150 g/milASTM D1922
Dart Drop 80.0 g/milASTM D1709
Film Tensile Strength at Break, MD 3200 psiASTM D882
Film Tensile Strength at Break, TD 3600 psiASTM D882
1% Secant Modulus, MD 33000 psiASTM D882
1% Secant Modulus, TD 30000 psiASTM D882
 
Optical PropertiesOriginal ValueComments
Haze 6.1 %ASTM D1003
Gloss 63 %@ 45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PFPCPQ9015 / 239836

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.