MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
KAY-CEL CORE U10 Unreinforced Polyurethane Foam
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: KAY-CEL CORE is a high-density polyurethane foam/fiberglass sandwich construction panel. It is used in many industries such as deerblinds, ice decking, marine, transportation, and many others due to its inherent strength and lack of water absorption.

Information provided by Kayco Composites LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 10.0 lb/ft³
Water Absorption 0.50 %
@Time 346000 sec
Volume Percent; ASTM D2842
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 0.300 ksi
Tensile Modulus 8.10 ksi
Flexural Strength 0.450 ksi
Flexural Modulus 10.7 ksi
Compressive Strength 0.330 ksi
Compressive Modulus 8.20 ksi
Shear Modulus 2.00 ksi
Shear Strength 0.170 ksi
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 1.2ASTM D1673
Dissipation Factor 0.0032
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.00 µin/in-°FASTM D696
Thermal Conductivity 0.310 - 0.350 BTU-in/hr-ft²-°FASTM D2326
Insulation R Value 2.86 - 3.24
Maximum Service Temperature, Air 200 °FDry

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKAYCO981 / 265377

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.