45% glass fiber, general purpose, heat stabilized Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep resistance and low moisture absorption are also characteristic of this resin. - Black: A-1145 HS BK 324 - Natural: A-1145 HS NT Markets/Uses: Automotive / Fuel Systems / Diesel Fuel Filtration Housings; Automotive / Mechanical & Structural Parts / Accumulator Piston Applications: Automotive Applications; Automotive Electronics; Automotive Under the Hood; Connectors; Housings; Industrial Applications; Industrial Parts; Machine/Mechanical Parts; Metal Replacement; Power/Other Tools; Valves/Valve Parts Features: Chemical Resistant; Creep Resistant; Good Dimensional Stability; Good Stiffness; High Heat Resistance; High Strength; High Temperature Strength; Low Moisture Absorption Injection notes: Storage: - Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding following the recommendations found in this datasheet and/or in the Amodel® processing guide. Information provided by Solvay Specialty Polymers. |