MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

RAMPF RAKU-TOOL® WB-1223 Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Polyurethane Board for Tools & Molds

Key Properties:

  • Low wear of milling tools
  • Very Resistant to amine
  • Most proven working board on the foundry market
  • Resistant to dry ice cleaning
  • Good abrasion resistance
Applications:
  • Foundry pattern plates
  • Hammer tools
  • Checking fixtures for metal parts

Information provided by © RAMPF Tooling Solutions GmbH & Co. KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 g/cc0.0441 lb/in³ASTM D-792
Storage Temperature 20.0 - 25.0 °C68.0 - 77.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 75 - 8575 - 85ASTM D-2240
Flexural Strength 70.0 - 80.0 MPa10200 - 11600 psiASTM D-790
Compressive Strength 60.0 - 70.0 MPa8700 - 10200 psiASTM D-695
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 - 85.0 µm/m-°C44.4 - 47.2 µin/in-°FASTM D-3386
Deflection Temperature at 0.46 MPa (66 psi) 80.0 - 90.0 °C176 - 194 °FASTM D-648
 
Descriptive Properties
ColorRed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRAMPF216 / 317816

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.