MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
HB Fuller Körapur 128 S Adhesive and sealant
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: Elastic one component adhesive and sealant for bonding in the manufacture of containers, vehicles, vehicle bodywork, air conditioning and heating equipment, metal-work, etc.
  • Good adhesion to primed and painted metals, aluminum and steel, wood and duroplastics
  • Good resistance to humidity and weathering
  • Overpaintable after curing
  • Resistant to temperatures from -40°C (-40°F) to +90°C (190°F) (up to +120°C (250°F) for short intervals)
  • Self-leveling
  • can be used with booster Köracur 110 S

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccDIN EN ISO 1183-1
Storage Temperature <= 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 40ISO 868 / DIN 53 505
Tensile Strength 1.50 MPaISO 868 / DIN 53 505
Elongation at Break >= 500 %ISO 868 / DIN 53 505
Tear Strength 5.00 kN/mISO 34 / DIN 53 515
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 35.0 °C
Minimum Service Temperature, Air 15.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 30.0 minSkin formation
 24.0 hour
@Thickness 3.00 mm
Shelf Life 9.00 MonthDrums
 12.0 MonthCartridges and sachets
 
Descriptive Properties
Base compoundPolyurethane one component, cures on exposure to humidity
ColorWhite, grey

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHBFULL105 / 316896

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.