MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Akrochem Naugard™ XL-1 Metal deactivator/Phenolic antioxidant
Categories: Other Engineering Material

Material Notes: Product Description: Naugard™ XL-1 metal deactivator is a unique antioxidant which incorporates a metal de-activation function in the same product. This product may be used where there is interference from metallic ions such as form residual polymer catalyst, inorganic pigments or mineral-filled polymers. This material can be used in a wide variety of polyolefinic and polystyrenic resins.

Features:

  • Dual functional antioxidant/metal de-activator
  • Non-discoloring
  • Synergistic with other antioxidants
CAS No: 693-36-7

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.12 g/cc1.12 g/cc
Molecular Weight 697 g/mol697 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point 170 - 180 °C338 - 356 °F
Flash Point 260 °C500 °FTOC
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 98 %
@Wavelength 425 nm
98 %
@Wavelength 425 nm
 
Descriptive Properties
AppearanceWhite to Off-white powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAKZCH509 / 315427

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.