MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Honeywell Acetonitrile, BC017-56 BioSyn® Low Water Content, Meets UV Specifications
Categories: Fluid

Material Notes: Suggested Application(s): Biosynthesis, Applications requiring low water content

Product Number : Package Size : Container Type
BC017-56 : 56L : SSPDS
BC017-200 : 200L : SSPDS
BC017-1250 : 1250L : SSPDS

Information provided by Honeywell

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.7822 g/cc
Viscosity 0.38 cP
Molecular Weight 41.05 g/mol
Vapor Pressure 88.8 torr
Surface Tension 19.1 dynes/cm
 
Thermal PropertiesOriginal ValueComments
Melting Point -43.8 °C
Boiling Point 81.6 °C
Flash Point 6.00 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.3434 - 1.3446
 
Descriptive Properties
Content<10 ppmWater by Karl Fischer Titration

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teijin Panlite® L-1225Y Standard (mold release/ice color grade) Polycarbonate Resin
Teijin Panlite® L-1250Y Standard (mold release/ice color grade) Polycarbonate Resin
Teijin Panlite® L-1250 Polycarbonate, Standard Grade
Teijin Panlite® L-1225L Standard (mold release/ice color grade) Polycarbonate Resin
Teijin Panlite® L-1225 Polycarbonate, Standard Grade

PHONWL191 / 179736

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.