LORD Thermoset SC-254 Blue encapsulant is a one-component, silicone encapsulant designed for coating and protecting electronic components. Features: exhibits low shrinkage and stress on components as it cures. provides controlled flow during application; ideal for conformal coatings. can be used on parts and devices that experience operating temperatures from -60°C to +200°C. All information provided by Lord. |