MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

UBE 3024GC6 PA12
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: Characteristic: Tube Coating. Quick connectors for fuel lines. Automotive grade. Property data reported dry as molded.

Information provided by UBE Industries, LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.24 g/cc0.0448 lb/in³ISO 1183-3
Moisture Absorption 0.400 %
@Time 86400 sec
0.400 %
@Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/inISO 294-4
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 235 °C
3.0 g/10 min
@Load 4.76 lb,
Temperature 455 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 110110ISO 2039-2
Tensile Strength, Yield 115 MPa16700 psiISO 527-1,2
Elongation at Break 7.0 %7.0 %ISO 527-1,2
Flexural Strength 170 MPa24700 psiISO 178
Flexural Modulus 5.80 GPa841 ksiISO 178
Charpy Impact, Notched  2.00 J/cm²
@Temperature -40.0 °C
9.52 ft-lb/in²
@Temperature -40.0 °F
ISO 179/1eA
 3.00 J/cm²
@Temperature 23.0 °C
14.3 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Taber Abrasion, mg/1000 Cycles 1212CS-17; ISO 9352
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear 0.300 µm/m-°C0.167 µin/in-°FISO 11359-2
Melting Point 178 °C352 °FISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 177 °C351 °FISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 160 °C320 °FISO 75-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PUBD9845 / 287308

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.