MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
A. Schulman BMC HT12-1026 Unsaturated Polyester Bulk Molding Compound
Categories: Polymer; Thermoset; Polyester, TS; Polyester (Thermoset) - Rigid

Material Notes: BMC HT12-1026 is a highly engineered Unsaturated Polyester Bulk Molding Compound developed for automotive under-hood applications. This compound is specified by Ford motor company for solenoid caps. Due to its excellent heat resistance and dimensional stability it performs well in automotive applications.

Information provided by Bulk Molding Compounds, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.75 - 1.95 g/ccMolded
Linear Mold Shrinkage 0.0015 - 0.0025 in/in
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 30 - 35
Tensile Strength 9800 - 11800 psi
Flexural Strength 19500 - 23500 psi
Flexural Modulus 1800 - 2000 ksi
Compressive Strength 21600 - 25600 psi
Izod Impact, Notched 5.10 - 7.10 ft-lb/in
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 347 - 397 V/milshort time
Arc Resistance 180 sec
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 425 - 500 °F
Flammability, UL94 HBThis product is not currently UL listed.
 
Processing PropertiesOriginal ValueComments
Processing Temperature 290 - 340 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 1026 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1026 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
A. Schulman BMC HT12-1027 Unsaturated Polyester Bulk Molding Compound
A. Schulman BMC HT12-1023L Unsaturated Polyester Bulk Molding Compound
A. Schulman BMC 100 Thermoset Polyester, GP

PBMC924 / 123388

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.