Base Polymer: Polyamide 6 Filler/Additive System: 50% glass fibers Special Features: High heat stabilized, easy release (demolding), Injection molding grade Typical Applications: Automotive, Machinery, Electrical and Electronic Information provided by Albis Plastics |