MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
HB Fuller HL9647 Adhesive
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: HL9647 is an isocyanate free hot melt moisture-curing adhesive. HL-9647 forms tough, heat resistant bonds after full cure. Cure time is a function of moisture availability and ambient temperatures. Typical cure times for HL-9647 at relative humidity of 30-60 % and ambient temperatures of 60 to 80 °F vary from 3 to 10 days depending on the substrate and coat weight. Open time of HL9647 vary depending on the substrate and method of application. In a thin film, open times range from 2 to 10 seconds and bead open time range from 30 to 60 seconds. HL9647 bonds well to nonpolar plastics, metals, paper, and wood.

Features and Benefits:

  • Isocyanate free
  • High heat resistance
  • High adhesion on a variety of substrates
  • High toughness
  • 100% solid

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.880 - 0.900 g/cc
Solids Content 100 %
Viscosity 13000 cP
@Temperature 149 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 - 10.0 secThin film
 30.0 - 60.0 secBead
 3.00 - 10.0 min
@Temperature 15.6 - 26.7 °C
30 to 60% R.H.
Shelf Life 6.00 Month
 
Descriptive Properties
ColorOff White
ConsistencyViscous LiquidSolid at Room Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHBFULL134 / 316925

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.