MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
BYK Gelwhite® GP Bentonite
Categories: Ceramic; Clay

Material Notes: Gelwhite GP is a highly purified montmorillonite refined from selectively mined natural white bentonite deposits. Gelwhite GP exhibits excellent thixotropy and enhances suspension stability and viscosity control. Gelwhite GP is also very effective at reducing syneresis in Home Care and Personal Care formulations.

Information provided by Southern Clay Products

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brightness 80 - 82 %
Particle Mesh Size 200 MeshWet, 0%
 200 MeshDry, >75%
pH 9.5 - 10.5
Viscosity >= 500 cPWater, 5% Slurry
 
Component Elements PropertiesOriginal ValueComments
Al2O3 17.7 %
CaO 2.2 %
Fe2O3 0.80 %
H2O, Water <= 8.0 %
K2O 0.10 %
MgO 3.2 %
Na2O 3.3 %
SiO2 66.5 %
 
Descriptive Properties
Color/FormFine White Powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BYK Gelwhite® L Bentonite
BYK Gelwhite® H Bentonite
BYK Laponite® D Magnesium Silicate
BYK Laponite® B Fluorosilicate
BYK Gelwhite® LS Rheology Modifier

PBYK054 / 185051

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.