Product Description: Mineralblend® PP-1600 is a medium flow talc filled homopolymer polypropylene compounds characterized by good impact strength, heat resistance and dimensional stability. Features: - Talc filled, 30%
- Good Impact Strength
- Good Heat Resistance
- Good dimensional stability
Uses:- Appliances Applications
- Electrical/Electronic Parts
Forms:Processing Method:Information provided by Colour Image Plastic Compound Sdn Bhd |