MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC LNP™ THERMOCOMP™ WX05456 PBT (Americas)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Mineral Filled

Material Notes: LNP THERMOCOMP WX05456 is a compound based on PBT containing Mineral.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.54 g/ccISO 1183
 1.546 g/ccASTM D792
Moisture Absorption 0.0500 %50% RH, 24 hrs; ASTM D570
 0.0700 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0147 cm/cm24 hrs; ISO 294
 0.015 cm/cm24 hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.015 cm/cm24 hrs; ASTM D955
 0.0151 cm/cm24 hrs; ISO 294
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 47.0 MPaISO 527
 48.0 MPaASTM D638
Elongation at Break 1.4 %ISO 527
 1.8 %ASTM D638
Flexural Strength 88.0 MPaISO 178
 90.0 MPaASTM D790
Flexural Modulus 4200 MPaISO 178
 4390 MPaISO 178/1A
Izod Impact, Notched 26.0 J/mASTM D256
Izod Impact, Unnotched 197 J/mASTM D4812
Izod Impact, Notched (ISO) 2.00 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 15.0 kJ/m²80*10*4; ISO 180/1U
Instrumented Impact Energy at Peak 7.00 JASTM D3763
Tangent Modulus 4220 MPa50 mm/min; ASTM D638
 4650 MPa1 mm/min; ISO 527
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 58.1 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E 831
 58.1 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 66.7 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E 831
 66.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 163 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 171 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 71.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Flammability, UL94 V-0
@Thickness 1.50 mm
UL 94 by SABIC-IP
 
Processing PropertiesOriginal ValueComments
Zone 1 230 - 245 °C
Zone 2 250 - 260 °C
Zone 3 265 - 275 °C
Melt Temperature 250 - 275 °C
Mold Temperature 80.0 - 95.0 °C
Drying Temperature 120 - 150 °C
Dry Time 4.00 hour
Moisture Content 0.020 %
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI20785 / 213921

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.