MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC LNP™ THERMOCOMP™ UX08325 PPA (Global)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA)

Material Notes: LNP THERMOCOMP UX08325 is PPA base glass fiber filled compounds, good for LDS (Laser direct structuring)application. Additional feature is high heat.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.55 g/ccASTM D792
Moisture Absorption 0.530 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0041 cm/cmSABIC method
Linear Mold Shrinkage, Transverse 0.0052 cm/cmSABIC method
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 125 MPa5 mm/min; ISO 527
 135 MPa5 mm/min; ASTM D638
Elongation at Break 1.6 %5 mm/min; ISO 527
 1.8 %5 mm/min; ASTM D638
Tensile Modulus 10880 MPa5 mm/min; ASTM D638
 11080 MPa1 mm/min; ISO 527
Flexural Strength 194 MPabrk, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Yield Strength 194 MPa2 mm/min; ISO 178
 197 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 9610 MPa2 mm/min; ISO 178
 9770 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Strain at Break 2.0 %2 mm/min; ISO 178
Izod Impact, Notched 31.0 J/mASTM D256
Izod Impact, Unnotched 351 J/mASTM D4812
Izod Impact, Notched (ISO) 2.00 kJ/m²80*10*4; ISO 180/1A
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 4.2
@Frequency 1e+9 Hz
ASTM D150
Dissipation Factor 0.010
@Frequency 1e+9 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 22.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 54.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 261 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 263 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Flammability, UL94 HB
@Thickness >=1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Zone 1 310 - 320 °C
Zone 2 315 - 325 °CInjection Molding
Zone 3 325 - 340 °C
Melt Temperature 315 - 330 °CInjection Molding
Mold Temperature 140 - 165 °C
Drying Temperature 120 - 150 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Moisture Content 0.15 %Injection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH92624 / 253748

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.