MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Covestro DESMODUR®MGQ33101 + BAYTEC®G30 + BAYTEC® XL B + PLASTICIZER V04 (Catalyst SD6-40) 40 A Polyurethane, MDI-PPG
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes:

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.930 g/ccPLASTICIZER V04
 1.01 g/ccBAYTEC® G30
 1.01 g/ccBAYTEC® XL B
 1.09 g/cc
 1.09 g/ccDESMODUR® MGQ33101
Viscosity 30 cPPLASTICIZER V04
 70 cPBAYTEC® XL B
 580 cPBAYTEC® G30
 2600 cPDESMODUR® MGQ33101
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 40DIN 53505
 40
@Temperature 80.0 °C
DIN 53505
 43
@Temperature -5.00 °C
DIN 53505
Tensile Strength at Break 6.00 MPaDIN 53504
Tensile Stress at Strain 0.300 MPa
@Strain 10 %
DIN 53504
Elongation at Break 435 %DIN 53504
100% Modulus 0.00110 GPa
@Strain 100 %
DIN 53504
200% Modulus 0.00200 GPa
@Strain 200 %
DIN 53504
300% Modulus 0.00330 GPa
@Strain 300 %
DIN 53504
Resilience 51[%]; DIN 53512
Tear Strength 34.2 pliwith nick; ISO 34-1
 120 pliwithout nick; ISO 34-1
Abrasion 215[mm3]; ISO 4649
Compression Set 8.0 %
@Temperature 70.0 °C,
Time 79200 sec
ISO 815-1
 
Processing PropertiesOriginal ValueComments
Processing Temperature 25.0 °CDESMODUR® MGQ33101
 25.0 °CBAYTEC® G30
 25.0 °CBAYTEC® XL B
 25.0 °CPLASTICIZER V04
Mold Temperature 80.0 °C
Pot Life 3.75 min
 
Descriptive Properties
AppearanceliquidDESMODUR® MGQ33101
 liquidBAYTEC® G30
 liquidBAYTEC® XL B
 liquidPLASTICIZER V04
Content100Parts by weight of prepolymer
 3Catalyst SD6-40 % / total (by weight), (catalyst at the head)
 45Parts by weight of PLASTICIZER V04
 65Parts by weight of BAYTEC® G30
 7.7Parts by weight of BAYTEC® XL B
 9.9-10.3%NCO

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCOVEST0489 / 202272

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.