System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Evonik VESTOPLAST® 704 Amorphous Polyalphaolefin
Categories:
Polymer
;
Thermoplastic
;
Polyalphaolefin
Material Notes:
VESTOPLAST 704 is a amorphous polyalphaolefin and propene-rich. Generally used as hot melt adhesives for labeling, sealing compositions, and spraying.
Key Words:
APAO
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
0.870
g/cc
@Temperature 23.0 °C
Viscosity
3000
-
4000
cP
@Temperature 190 °C
melt, rotational viscometer; DIN 53 019
Molecular Weight
8000
g/mol
Mn; GPC
35000
g/mol
Mw; GPC
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
0.500
MPa
DIN EN ISO 527-3
Elongation at Break
100 %
DIN EN ISO 527-3
Shear Modulus
0.00750
GPa
@Temperature 23.0 °C
DIN EN ISO 6721-2
Penetration
18 - 28
@Thickness 0.100 mm
needle 100/25/5; DIN 52 010
Thermal Properties
Original Value
Comments
Maximum Service Temperature, Air
75.0
-
80.0
°C
under load 5 °C/h, weight 450g; Degussa Method
Glass Transition Temp, Tg
-36.0
°C
DSC
Ring & Ball Softening Point
100
-
110
°C
DIN 52 011
Descriptive Properties
Open Time (sec)
80
Degussa Method
Setting Time (sec)
1
Degussa Method
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Evonik VESTOPLAST® 828 Amorphous Polyalphaolefin
Evonik VESTOPLAST® 703 Amorphous Polyalphaolefin
Evonik VESTOPLAST® 888 Amorphous Polyalphaolefin
Evonik VESTOPLAST® 608 Amorphous Polyalphaolefin
Evonik VESTOPLAST® 792 Amorphous Polyalphaolefin
PHUMB418 / 81420
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.