MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
American Elements Bismuth Oxide Nanopowder
Categories: Ceramic; Oxide

Material Notes: General Description

Bismuth Oxide ( BiO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles. Nanoscale Bismuth Oxide Particles are typically 20-80 nanometers (nm) with specific surface area (SSA) in the 10 – 50 m 2 /g range and also available in with an average particle size of 100 nm range with a specific surface area of approximately 7- 10 m 2 /g. Nano Bismuth Oxide Particles are also available in ultra high purity and high purity, transparent, and coated and dispersed forms. Applications for Bismuth Oxide Nanocrystals include various electrochemical uses, such as in the electrolyte or cathode of solid oxide fuel cells (SOFC), in bio-medical and cancer imaging and for other photoconductive characteristics in thin films.

Key Words: Formula: Bi2O3; CAS Number: 1304-76-3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Particle Size 0.020 - 0.080 µm
 0.10 µm
Specific Surface Area 7.0 - 10 m²/g
 10 - 50 m²/g
Molecular Weight 465.96 g/mol
 
Descriptive Properties
AppearanceYellow Powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
MV Labs BI800 Bi2O3 Bismuth oxide
Bismuth Oxide, Bi2O3 (Bismite)

EJAMER11 / 5494

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.