MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ascend Performance Materials HiDura™ MED AI1 NT0861 PA66-I
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Impact Grade

Material Notes: HiDura MED AI1 NT0861 is a high impact-modified PA66 resin designed for healthcare applications. The product provides all the processing and performance advantages of PA66 with excellent impact strength even at low temperatures and can be easily colored. This product offers a combination of engineering properties characterized by excellent toughness and flexibility; high melt point; and resistance to many chemicals including disinfectants. The product is compliant to ISO 10993-5 and ISO 10993-10. It exhibits good property retention after most sterilization methods.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³DAM; ISO 1183
Water Absorption 1.0 %
@Time 86400 sec
1.0 %
@Time 24.0 hour
DAM; ISO 62
Moisture Absorption at Equilibrium 2.1 %2.1 %DAM to 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.018 cm/cm
@Thickness 2.00 mm
0.018 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.016 cm/cm
@Thickness 2.00 mm
0.016 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 39.0 MPa5660 psi50% RH; ISO 527-2
 43.0 MPa6240 psiDAM; ISO 527-2
Tensile Strength, Yield 35.0 MPa5080 psi50% RH; ISO 527-2
 50.0 MPa7250 psiDAM; ISO 527-2
Elongation at Break 50 %50 %DAM; ISO 527-2
 175 %175 %50% RH; ISO 527-2
Tensile Modulus 1.40 GPa203 ksi50% RH; ISO 527-2
 2.20 GPa319 ksiDAM; ISO 527-2
Flexural Strength 17.0 MPa2470 psi50% RH; ISO 178
 53.0 MPa7690 psiDAM; ISO 178
Flexural Modulus 0.500 GPa72.5 ksi50% RH; ISO 178
 1.80 GPa261 ksiDAM; ISO 178
Izod Impact, Notched (ISO)  29.0 kJ/m²
@Temperature -30.0 °C
13.8 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 180/1A
 40.0 kJ/m²
@Temperature -30.0 °C
19.0 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 180/1A
 78.0 kJ/m²
@Temperature 23.0 °C
37.1 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
 88.0 kJ/m²
@Temperature 23.0 °C
41.9 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 180/1A
Charpy Impact Unnotched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
50% RH; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
DAM; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
50% RH; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
DAM; ISO 179/1eU
Charpy Impact, Notched  2.50 J/cm²
@Temperature -30.0 °C
11.9 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 179/1eA
 3.50 J/cm²
@Temperature -30.0 °C
16.7 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eA
 7.60 J/cm²
@Temperature 23.0 °C
36.2 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 11.0 J/cm²
@Temperature 23.0 °C
52.3 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 168 µm/m-°C
@Thickness 2.00 mm,
Temperature 35.0 - 55.0 °C
93.3 µin/in-°F
@Thickness 0.0787 in,
Temperature 95.0 - 131 °F
DAM; ISO 11359-2
CTE, linear, Transverse to Flow 149 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
82.8 µin/in-°F
@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
DAM; ISO 11359-2
Melting Point 260 °C500 °FDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 145 °C293 °FUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 58.0 °C136 °FUnannealed; DAM; ISO 75-2/A
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 280 - 310 °C536 - 590 °FInjection
Middle Barrel Temperature 280 - 310 °C536 - 590 °FInjection
Front Barrel Temperature 280 - 310 °C536 - 590 °FInjection
Nozzle Temperature 280 - 310 °C536 - 590 °FInjection
Melt Temperature 285 - 305 °C545 - 581 °FInjection
Mold Temperature 65.0 - 95.0 °C149 - 203 °FInjection
Drying Temperature 80.0 °C176 °FInjection
Dry Time 4.00 hour4.00 hourInjection
 
Descriptive Properties
AdditiveLubricant
 Release agent
Agency RatingsBSE/TSE Compliant
AppearanceNatural Color
FeaturesAcoustical Barrier Properties
 Bromine Free
 Chemical Resistant
 Corrosion Resistant
 Crack Resistant
 Ductile
 Good Colorability
 Good Impact Strength
 Good Processability
 Good Surface Finish
 Halogen Content, None
 High Toughness
 Homopolymer
 Impact Modified
 Low Temperature Impact Resistance
 Low Temperature Toughness
 Lubricated
 Solvent Resistant
 Ultra High Impact Resistance
FormsPellets
Processing MethodInjection Molding
 Profile Extrusion
RegionNorth America, Europe, Asia Pacific

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASCE8504 / 296323

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.