MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Mocom (ALBIS) ALCOM® TCD PA6 5060 FR 15090 Nylon 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Base Polymer: Polyamide 6

Filler/Additive System: Special filler

Special Features: Thermal conductive, electrically insulating, heat ageing stabilization, halogen-free flame retardant, opaque

Market Segment: Automotive, Machinery, Electrical and Electronic, Lighting radiator systems, cooling system

Application Area: Radiator systems, cooling system

Typical Applications: Housings, functional components, plugs/connectors, lamp sockets

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.63 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0070 - 0.011 cm/cm
@Time 86400 sec
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0050 - 0.0090 cm/cm
@Time 86400 sec
ISO 294-4
Spiral Flow 230 cm
@Thickness 2.00 mm
Storage Temperature <= 30.0 °Cdry, protected from light
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 80.0 MPaISO 527
Elongation at Break 1.5 %ISO 527
Tensile Modulus 10000 MPaISO 527
Flexural Strength 140 MPaISO 178
Flexural Modulus 9500 MPaISO 178
Charpy Impact Unnotched 30.0 kJ/m²ISO 179/1eU
 
Electrical PropertiesOriginal ValueComments
Surface Resistance >= 1.00e+12 ohmDIN EN 62631-3-2
Dielectric Strength 27.0 kV/mmIEC 20243-1
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.49 J/g-°C
Thermal Conductivity 1.00 W/m-KISO 22007-2
 1.00 W/m-Kthrough-plane; ASTM E 1461
 1.50 W/m-Kin-plane; ASTM E 1461
Melting Point 220 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 175 °CISO 75-1/-2
Vicat Softening Point 215 °CB50; ISO 306
Flammability, UL94 V-2
@Thickness 1.50 mm
Glow Wire Flammability Index 960 °C
@Thickness 1.00 mm
passed; DIN EN 60695
 
Processing PropertiesOriginal ValueComments
Melt Temperature 270 - 300 °CInjection molding
Mold Temperature >= 100 °CInjection molding
Drying Temperature 80.0 °C
@Time 7200 - 43200 sec
in a dry air (desiccant) dryer
 
Descriptive Properties
Base PolymerPolyamide 6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PALBIS8202 / 242261

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.