Notes: Monprene CP-19318 is a high performance thermoplastic elastomer designed for a variety of consumer product applications requiring a soft, rubber-like feel. Monprene CP-19318 is a transparent, lubricated, low hardness, low density grade that is suitable for injection molding. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Features: High Flow; Low Density; Low Hardness; Low Specific Gravity; Lubricated; Slip; Without Fillers Uses: Consumer Applications; Handles; Writing instruments RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Injection Molding Information provided by Teknor Apex |