MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

3H Vinacom PVC Compound Flame Retardant
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Extruded

Material Notes: Description: The PVC compound grades are included insulation and sheath application of wire and cable with temperature rating of less then 1050C and conform to the international and Vietnam standards such as ASTM D1505, UL 62, UL 94, IEC 60502, IEC 60227, TCVN 5935, TCVN 6610, RoSH directive 2002/95/EC and its amending directives. Beside that special PVC properties are available upon customers requirement. There also available some grades are produced with characteristics of durableness, termite resistance, heat resistance, flamable resistance, dull and gloss surface.

Applications: PVC compound is commonly used for a wide range of applications in sectors even very different from each other. The compounds are used for both rigid and flexible formulations. Main flexible applications are spiral tubes, gaskets, crystal shoes and technical tubes, shoes, films, plates, medical and surgical devices and wires and cables (electric, telephone systems, telecommunications industry and plugs) are produced with excellent physical and technical performance. Rigid applications they are mainly used for raceways, rolling shutters and window profiles, electric and hydraulic connections, spiral tubes and medical equipment, electronic equipment (office automation, conduits, electrical boxes).

Information provided by 3H Vinacom

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.48 - 1.52 g/cc0.0535 - 0.0549 lb/in³IEC 60811
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 86 - 9086 - 90ISO 868
Tensile Strength >= 0.125 MPa>= 18.1 psiIEC 60811
 0.03114 MPa
@Temperature 100 °C,
Time 605000 sec
4.516 psi
@Temperature 212 °F,
Time 168 hour
After Aging; IEC 60811
Elongation at Break >= 150 %>= 150 %IEC 60811
 37.5 %
@Temperature 100 °C,
Time 605000 sec
37.5 %
@Temperature 212 °F,
Time 168 hour
After Aging; IEC 60811
Heat Distortion <= 50 %<= 50 %IEC 60811
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 60502
 
Thermal PropertiesMetricEnglishComments
Oxygen Index >= 30 %>= 30 %KSM 3032
 
Processing PropertiesMetricEnglishComments
Processing Temperature 145 °C293 °FC1
 150 °C302 °FC2
 155 °C311 °FC3
 160 °C320 °FC4
 165 °C329 °FC5
 165 °C329 °FNeck
Die Temperature 170 °C338 °F
Head Temperature 165 °C329 °F
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
CompositionCadmium
 Chromium VI
 Lead
 Mercury
 PBBs / PBDEs

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PVINAC001 / 249350

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.