Glass fiber-reinforced and inorganically filled polyester molding compound (UP) in various colors. Outstanding mechanical strength similar to BMC/SMC, very good electrical isolation properties and dimensional stability, excellent processability. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 2002/96 (WEEE) and 2006/122 (PFOS). Processing: Injection, Transfer and Compression molding. Applications: Connectors, Bobbins, Housings and Mounting plates Information provided by the Raschig Group |