MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Copper Alloy, UNS C70620, M10 Temper, Forgings
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: As Hot Forged - Air Cooled

Typical uses: Cu-Ni forgings for sea water exposure

Applicable Specifications: ASME SB111; Condenser & Heat Exchanger Tube with Integral Fins – ASTM B956/B956M; Die – ASTM B283/B283M; Heat Exchanger Tube – Welded ASTM B543/B543M; Pipe – Welded ASTM B467, ASTM B466/B466M, Welded ASTM B608; Plate – ASTM B171/B171M; Rod & Bar – ASTM B151/B151M; Rod, Bar & Shapes – ASTM B124/B124M; Sheet, Strip, Roller Bar & Plate – ASTM B122/B122M; Tube – ASTM B359/B359M, ASTM B466/B466M, ASTM B111/B111M, ASTM B395/B395M; Tube, water – Welded ASTM B552

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 40.0 ksi
 >= 45.0 ksi
@Thickness 152 mm
Tensile Strength, Yield >= 15.0 ksi0.2% Offset
 >= 18.0 ksi
@Thickness 152 mm
Elongation at Break >= 30 %
 >= 30 %
@Thickness 152 mm
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.050 %
Copper, Cu >= 86.5 %
Iron, Fe 1.0 - 1.8 %
Lead, Pb <= 0.020 %
Manganese, Mn <= 1.0 %
Nickel, Ni 9.0 - 11 %
Phosphorus, P <= 0.020 %
Sulfur, S <= 0.020 %
Zinc, Zn <= 0.50 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC70620x1 / 292447

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.